The pattern of fracture by impact penetration test and tensile fatigue test of thermite welding with stereoscan was observed,and the component of defect with energy spectrum was analyed.
观缺陷主要包括
孔和夹杂,其中
孔由
气孔和
缩孔组成,夹杂物按形态和尺
分为团簇状夹杂、锥状夹杂、粒状夹杂、积聚物夹杂、丝状夹杂和混合形夹杂。